@prefix dcat: <http://www.w3.org/ns/dcat#> .
@prefix dcterms: <http://purl.org/dc/terms/> .
@prefix foaf: <http://xmlns.com/foaf/0.1/> .
@prefix prov: <http://www.w3.org/ns/prov#> .

<https://datagraph.stage.matportal.org/id/dataset/nanoindentation-cuzn23si2-5-imws> a dcat:Dataset ;
  dcterms:title "Nanoindentation_CuZn23Si2.5_IMWS" ;
  dcterms:description "Nanoindentation_CuZn23Si2.5_IMWS is a MatPortal dataset catalogue entry listed under KupferDigital, catalogued under source association 910c1a74-6a71-4531-a4eb-0b7e4dcbc166. It includes 3 linked resources with formats such as PNG, opju, image/bmp, including FEMBau02_CuZn23Si2_5_modulus Graph.png, FEMBau02_CuZn23Si2_5.opju, FEMBau02_CuZn23Si2_5_pos.bmp. Review the linked source for license and reuse conditions. The original short source note was: hardness and modulus. It is published in MatPortal by admin for dataset discovery, linked-data browsing, and assistant/RAG indexing." ;
  dcterms:identifier "684ce496-b770-4b74-9e78-a9a406f19110" ;
  dcterms:license "License not specified" ;
  dcterms:publisher "[{\"email\": \"\", \"identifier\": \"\", \"name\": \"IMWS\", \"type\": \"\", \"uri\": \"https://ckan.kupferdigital.org/organization/25667935-76d7-4a0f-9028-b67a2bef1599\", \"url\": \"\"}]" ;
  prov:wasDerivedFrom "Harvested from Platform MaterialDigital CKAN Action API without credentials. "
  ; dcat:distribution <https://datagraph.stage.matportal.org/id/distribution/nanoindentation-cuzn23si2-5-imws/resource_72aece9942dc07f4>
  ; dcat:distribution <https://datagraph.stage.matportal.org/id/distribution/nanoindentation-cuzn23si2-5-imws/resource_74b03737b09b4591>
  ; dcat:distribution <https://datagraph.stage.matportal.org/id/distribution/nanoindentation-cuzn23si2-5-imws/resource_e3a0972083f10834> .

<https://datagraph.stage.matportal.org/id/distribution/nanoindentation-cuzn23si2-5-imws/resource_72aece9942dc07f4> a dcat:Distribution ;
  dcterms:title "FEMBau02_CuZn23Si2_5_modulus Graph.png" ;
  dcat:accessURL <https://ckan.kupferdigital.org/dataset/684ce496-b770-4b74-9e78-a9a406f19110/resource/168396f8-0d21-46dd-8c86-321675223c97/download/fembau02_cuzn23si2_5_modulus-graph.png> ;
  dcterms:format "PNG" .

<https://datagraph.stage.matportal.org/id/distribution/nanoindentation-cuzn23si2-5-imws/resource_74b03737b09b4591> a dcat:Distribution ;
  dcterms:title "FEMBau02_CuZn23Si2_5.opju" ;
  dcat:accessURL <https://ckan.kupferdigital.org/dataset/684ce496-b770-4b74-9e78-a9a406f19110/resource/5bfe3c1c-e65a-4af2-af69-1691684bd759/download/fembau02_cuzn23si2_5.opju> ;
  dcterms:format "opju" .

<https://datagraph.stage.matportal.org/id/distribution/nanoindentation-cuzn23si2-5-imws/resource_e3a0972083f10834> a dcat:Distribution ;
  dcterms:title "FEMBau02_CuZn23Si2_5_pos.bmp" ;
  dcat:accessURL <https://ckan.kupferdigital.org/dataset/684ce496-b770-4b74-9e78-a9a406f19110/resource/fb5848a1-60cf-4d4f-a5ae-287a362884e1/download/fembau02_cuzn23si2_5_pos.bmp> ;
  dcterms:format "image/bmp" .